Dear customers:
Thank you for using our company's amtique mirror,according to the chemical principle,
plating silver layer and copper layer on the high quality float glass or tinted float
glass,and then putting double coated for protection,drying at lasr. The mirror surface
is clear and bright,giving distince and life like image.The plating layer is rigid and
bond and the protective layer impregnable with godd erosion-resistance.
please pay attention to the following when using;
1.Antique mirror only 72 hours after the production can be or others processing,please
do not scratch the back of the mirror.
2.Please use high grade cutting fluid for cutting.
3.Edging should be sure getting enough cooling water,update perioclically(12h/time,best to
use deionized water for producing )use good edge grinding wheel,dc not dry grind or destory
the back paint.
4.Washing immediately after grinding,drying and keep in wentilated place. best to use edging seal
on the edge
5.Avoid acid or base corroding when installiing the mirror,please use prefessional mirror glue
6.Back paint do not touch rubber latex directly, also can not put others fluid on the back
paint long time.
7.Please keep the antique mirror in the wentilated place inside,can not put in in outside exposed
place and touch acidoid acidic material, basic compounds,liquor especially hydrofluoric acid.
Warm promt :if you have any problems above, please feel free to tell us,we will reply you asap